Electrodes For Manual Arc Welding. The Chemical Composition Of The Melted Metal: Carbon Not More Than 0.12%; Manganese 0.35-0.70%; Silicon 0.09-0.25%; Sulfur, Not More Than 0.04%; Phosphorus, Not More Than 0.045%. The Consumption Of Electrodes Per 1 Kg Of A Melted Metal 1.7 Kg. Surfacing Coefficient 8.5 G/A*H. Diameter 3 Mm. Productivity, 1.2 Kg/H. Gost 9466-75., Galled Prickly Wire - An Effective Method Of Protecting The Territories From The Penetration Of Outsiders. The View Of The Wire Is Prickly. Coating - Zinc. Material - Metal. Color Is White. The Type Of Grid Is Enclosing. Gost 285-69., The Pipe Is Profile. Section 40X40 Mm. The Thickness Is 2 Mm. Length 3 M. Width 40 Mm. Height 40 Mm. Form - Square. The Main Material Is Steel. Coating - Without Coating. Gost 30245-2012.